International Export Desk Welding Filler Wires & Alloy Consumables Supplier from India — A Venture of Creative Piping Solutions Pvt. Ltd.

Monel Filler Wires Supplier — Monel 400 (ERNiCu-7) & Monel 67 Welding Wire

Nickel-Copper (ERNiCu-7 / Filler Metal 60) and Copper-Nickel (Monel 67) welding filler wires engineered for marine splash-zone sheathing, hydrofluoric acid alkylation units, desalination plants and brine evaporators.

AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67) UNS: UNS N04060 (ERNiCu-7) / UNS C71580 (Filler 67) Werkstoff: 2.4377 (Base: 2.4360) GTAW (TIG), GMAW (MIG), SAW
Monel 400 ERNiCu-7 and Monel 67 welding filler wires
Monel 400 (AWS A5.14 ERNiCu-7) and Monel 67 TIG rods and MIG spooled welding wires.
Nickel Alloy Filler Wires

Nickel-Copper Welding Consumables for Flowing Seawater, Splash Zones & Hydrofluoric Acid

Monel Filler Wires encompass two essential nickel-copper welding consumables: Monel Filler Metal 60 (AWS A5.14 ERNiCu-7 / UNS N04060) for welding Monel 400 (UNS N04400) and Monel R-405, and Monel Filler Metal 67 (70Cu-30Ni / ERCuNi type) for joining copper-nickel alloys and dissimilar Monel-to-CuNi marine systems. Monel 400 filler wire contains ~65% Nickel, ~30% Copper, 3.5% Manganese and 1.5–3.0% Titanium, where titanium acts as a critical deoxidizer and nitrogen scavenger to eliminate porosity during arc welding.

Monel 400 weld deposits exhibit extraordinary resistance to high-velocity flowing seawater, marine splash-zone corrosion on offshore platform risers and legs, brackish water, chlorinated solvents, alkalies and hydrofluoric (HF) acid in refinery alkylation units.

AWS Classification AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67)
EN / ISO Classification EN ISO 18274 S Ni 4060 (NiCu30Mn3Ti)
UNS / Werkstoff Nr. UNS N04060 (ERNiCu-7) / UNS C71580 (Filler 67) / 2.4377 (Base: 2.4360)
Welding Processes GTAW (TIG), GMAW (MIG), SAW

Alloy Identification, Standards & Supply Specifications

When overlaying or welding Monel 400 directly onto carbon steel where iron dilution exceeds 10–15%, apply a pure nickel (ERNi-1 / Filler Metal 61) or ERNiCr-3 buffer layer first to prevent copper-induced hot cracking.

Technical Product Specification Summary — Monel 400 & Monel 67 Filler Wires
Product Designation Monel 400 & Monel 67 Filler Wires (TIG Welding Rod / MIG Spooled Wire)
AWS / ASME Classification AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67)
EN / ISO Classification EN ISO 18274 S Ni 4060 (NiCu30Mn3Ti)
UNS Designation & Werkstoff Nr. UNS N04060 (ERNiCu-7) / UNS C71580 (Filler 67) • W.Nr. 2.4377 (Base: 2.4360)
Compatible Base Materials Monel Alloy 400 (UNS N04400 / W.Nr. 2.4360), Monel R-405 (N04405), Copper-Nickel alloys (70/30 and 90/10 with Monel 67), and clad Monel 400 vessels (with appropriate nickel buffer).
Supported Welding Processes GTAW (TIG), GMAW (MIG), SAW
Shielding Gas Recommendations 100% Argon (GTAW); Argon or Argon + Helium (GMAW)
Available Wire Diameters MIG Spools: 0.8mm (.030"), 0.9mm (.035"), 1.0mm (.040"), 1.2mm (.045"), 1.6mm (1/16")
TIG Cut-Length Rods: 1.2mm, 1.6mm (1/16"), 2.0mm, 2.4mm (3/32"), 3.2mm (1/8"), 4.0mm (5/32") × 914mm (36") / 1000mm
Packaging & Storage TIG Rods: 5 kg / 10 kg moisture-resistant tubular plastic packs in export master cartons.
MIG Wire: 12.5 kg / 15 kg precision layer-wound BS300 / S200 spools sealed in VCI polyethylene film.
Storage: Store in a dry, temperature-controlled indoor store (+10°C to +40°C, <60% RH) in original sealed packaging.

Chemical Composition Specification (AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67))

The table below specifies the standard wire chemical composition limits in weight percent (wt.%). Single values represent maximum permissible limits unless stated otherwise:

Chemical Composition Limits — Monel 400 & Monel 67 Filler Wires
Element Verified Specification Limit (wt.%) Metallurgical Function in Weld Metal
Nickel + Cobalt (Ni+Co) 62.0 – 69.0 (ERNiCu-7) Primary matrix providing alkali, HF acid and chloride SCC resistance
Copper (Cu) Remainder (~28 – 32%) Solid-solution partner enhancing seawater and reducing-acid resistance
Manganese (Mn) 4.0 max (Typical: 3.0 – 4.0) Prevents hot microfissuring and assists weld pool deoxidation
Titanium (Ti) 1.5 – 3.0 Essential deoxidizer/denitrider preventing weld metal gas porosity
Iron (Fe) 2.5 max Controlled iron enhances cavitation-erosion resistance
Silicon (Si) 1.25 max Fluidity and deoxidation control
Carbon (C) 0.15 max Standard limit per AWS A5.14
Aluminum (Al) 1.25 max Auxiliary deoxidizer
Phosphorus (P) & Sulfur (S) P ≤ 0.020, S ≤ 0.015 Strict impurity limits

Mechanical & Physical Properties

The values below distinguish between minimum AWS/ISO classification requirements for all-weld-metal test assemblies and typical as-welded deposited weld metal benchmarks:

Mechanical & Physical Property Reference — Monel 400 & Monel 67 Filler Wires
Property Value Unit Specification / Reference Basis
Tensile Strength ≥ 480 (Typical: 510 – 550) MPa AWS A5.14 ERNiCu-7 Minimum / Typical
Yield Strength (0.2% Offset) ≥ 200 (Typical: 230 – 270) MPa Typical As-Welded GTAW Deposit
Elongation ≥ 30 (Typical: 35 – 40) % AWS A5.14 Minimum in 4D
Density 8.80 g/cm³ Physical Property Reference
Melting Range 1300 – 1350 °C Physical Property Reference
Technical Verification Statement: Standard limits above reflect published AWS / ASME / EN ISO classification specifications and typical deposited weld metal properties. Actual heat-specific test results depend on wire diameter, batch chemistry and welding procedure parameters. Contact us for confirmed product specifications and available technical documentation.

Product Comparison: Monel 400 (ERNiCu-7 / FM 60) vs. Monel 67 Filler Wire

Comparison of Monel 400 (Filler Metal 60) and Monel 67 Filler Wires
Attribute Monel 400 / Filler Metal 60 (AWS A5.14 ERNiCu-7) Monel 67 Filler Wire (AWS A5.7 ERCuNi Type)
Nominal Alloy Balance ~65% Nickel – 30% Copper – 3.5% Mn – 2.2% Ti ~67% Copper – 30% Nickel – 0.6% Fe – 0.8% Mn – 0.35% Ti
Primary Base Metals Monel 400 (UNS N04400) & Monel R-405 70/30 & 90/10 Cupro-Nickel and CuNi-to-Monel 400 joints
Minimum Tensile Strength 480 MPa (70 ksi) 345 MPa (50 ksi)
Core Industrial Duty Offshore riser splash-zone sheathing, HF acid alkylation, salt evaporators Seawater desalination piping, marine condensers, ship hulls

Corrosion Resistance, Welding Considerations & Industrial Applications

Monel 400 filler wire offers unmatched durability in the splash and tidal zones of offshore oil & gas platforms, where alternating wet and dry aerated seawater rapidly corrodes steel. In refinery hydrofluoric (HF) acid alkylation units, ERNiCu-7 is the standard consumable for welding Monel 400 fractionator columns, valves and piping.

Typical Industrial Applications

  • Offshore oil & gas platform riser and jacket splash-zone Monel 400 sheathing in the Arabian Gulf and North Sea
  • Refinery hydrofluoric (HF) acid alkylation columns, reboilers, valves and piping
  • Multi-Stage Flash (MSF) desalination brine heaters, demisters and vacuum salt evaporators
  • Marine propeller shafts, seawater pump impellers and naval hull fittings
  • Uranium refining and fluorination chemical processing equipment

International Enquiry Destinations

FillerWires welcomes B2B export enquiries for Monel 400 & Monel 67 Filler Wires from EPC contractors, process equipment fabricators, shipyards and distributors across the following priority countries and industrial cities:

International Enquiry Destinations for Monel 400 & Monel 67 Filler Wires
Target Country Relevant Industrial Cities & Ports Typical Regional Sector Demand
Qatar & United Arab Emirates Doha, Ras Laffan, Abu Dhabi, Dubai, Sharjah, Fujairah Offshore platform splash-zone sheathing & LNG marine systems
Saudi Arabia & Kuwait Dammam, Jubail, Ras Tanura, Yanbu, Ahmadi, Shuaiba Refinery HF alkylation units & offshore jackets
Oman & Bahrain Muscat, Sohar, Duqm, Salalah, Manama, Hidd, Sitra Desalination brine heaters & shiprepair drydocks
United States & United Kingdom Houston, Corpus Christi, New Orleans, Aberdeen, Southampton Gulf Coast HF alkylation refineries & offshore rigs
Italy, Netherlands & Norway Genoa, Milan, Venice, Rotterdam, Stavanger, Bergen Marine heat exchangers, refineries & offshore platforms
Singapore, Sri Lanka & Peru Jurong, Tuas, Colombo, Callao, Talara FPSO marine conversion & refinery maintenance

Frequently Asked Questions — Monel 400 & Monel 67 Filler Wires

Technical questions and answers regarding classification, base metal compatibility, welding parameters and procurement for Monel 400 & Monel 67 Filler Wires:

Monel 400 & Monel 67 Filler Wires is classified under AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67) and EN ISO 18274 S Ni 4060 (NiCu30Mn3Ti) (UNS UNS N04060 (ERNiCu-7) / UNS C71580 (Filler 67), Werkstoff Nr. 2.4377 (Base: 2.4360)). Contact us for confirmed product specifications and available technical documentation.

Monel 400 & Monel 67 Filler Wires (AWS A5.14 ERNiCu-7 (Monel 60) / AWS A5.7 ERCuNi (Monel 67)) is engineered for welding Monel Alloy 400 (UNS N04400 / W.Nr. 2.4360), Monel R-405 (N04405), Copper-Nickel alloys (70/30 and 90/10 with Monel 67), and clad Monel 400 vessels (with appropriate nickel buffer).

Monel 400 & Monel 67 Filler Wires is supplied for GTAW (TIG), GMAW (MIG), SAW as precision layer-wound MIG spools (0.8mm, 0.9mm, 1.0mm, 1.2mm, 1.6mm) and straight cut-length TIG rods (1.2mm, 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm in 914mm / 36-inch and 1000mm lengths). Recommended shielding gas: 100% Argon (GTAW); Argon or Argon + Helium (GMAW).

Monel 400 filler wire offers unmatched durability in the splash and tidal zones of offshore oil & gas platforms, where alternating wet and dry aerated seawater rapidly corrodes steel. In refinery hydrofluoric (HF) acid alkylation units, ERNiCu-7 is the standard consumable for welding Monel 400 fractionator columns, valves and piping. Typical applications include: Offshore oil & gas platform riser and jacket splash-zone Monel 400 sheathing in the Arabian Gulf and North Sea; Refinery hydrofluoric (HF) acid alkylation columns, reboilers, valves and piping; Multi-Stage Flash (MSF) desalination brine heaters, demisters and vacuum salt evaporators.

Direct Export & Procurement Desk

International B2B Technical Enquiry & Quotation Request

Submit your alloy grade, AWS/ISO classification, diameter, welding process and delivery destination. Our technical export team in Mumbai responds to enquiries from the Middle East, GCC, USA, UK, Europe, Singapore, Sri Lanka, South Africa, Peru and global markets.

Section A – Contact Information
Section B – Product Requirements
Multiple grades accepted. If unsure of the exact classification, enter “Not sure – Need technical assistance”.
Section C – Quantity Requirements
Section D – Technical and Project Details
To share technical specifications or supporting documents, please email info@fillerwires.com directly.
Direct Email: info@fillerwires.com | Tel/WhatsApp: +91 7045 212 326

Ready to Source Certified Welding Filler Wires for Your Next Project?

Connect with our international export team in Mumbai for technical datasheets, alloy availability, packaging options and competitive CIF/FOB quotations for the Middle East, GCC, USA, UK, Europe and global markets.