Cupro Nickel 70/30 Filler Wire Supplier — AWS A5.7 ERCuNi Welding Wire
70% Copper / 30% Nickel titanium-deoxidized filler metal (AWS A5.7 ERCuNi / UNS C71580) engineered for welding 70/30 and 90/10 copper-nickel seawater piping, desalination evaporators and marine heat exchangers.
AWS A5.7 ERCuNi — The Benchmark 70/30 Copper-Nickel Marine Filler Metal
Cupro Nickel 70/30 Filler Wire (classified under AWS A5.7 / ASME SFA-5.7 ERCuNi and EN ISO 24373 S Cu 7158) is a nominal 67% Copper – 30% Nickel solid welding wire containing controlled iron (0.40–0.75%), manganese (1.0% max) and titanium (0.20–0.50%). In flowing seawater and hot brine, the iron-modified cupro-nickel matrix forms a tough, self-healing protective surface film that resists impingement erosion, cavitation, biofouling and chloride crevice corrosion.
Under international marine welding codes, 70/30 ERCuNi filler wire is used to weld both 70/30 (C71500) AND 90/10 (C70600) copper-nickel base metals. Using 70/30 filler metal on 90/10 piping ensures that the smaller weld metal area is slightly cathodic (more noble) compared to the surrounding 90/10 pipe wall, preventing preferential galvanic corrosion of the weld seam in seawater.
Alloy Identification, Standards & Supply Specifications
Titanium (0.20–0.50%) is deliberately alloyed into ERCuNi filler wire to react with dissolved oxygen and nitrogen in the molten weld pool, eliminating porosity during single- and multi-pass GTAW and GMAW welding.
| Product Designation | Cupro Nickel 70/30 Filler Wire (TIG Welding Rod / MIG Spooled Wire) |
|---|---|
| AWS / ASME Classification | AWS A5.7 / ASME SFA-5.7 ERCuNi |
| EN / ISO Classification | EN ISO 24373 S Cu 7158 (CuNi30Mn1FeTi) |
| UNS Designation & Werkstoff Nr. | UNS C71580 / C71581 • W.Nr. 2.0837 (CuNi30Fe) |
| Compatible Base Materials | Copper-Nickel 70/30 (UNS C71500 / CuNi30Mn1Fe), Copper-Nickel 90/10 (UNS C70600 / CuNi10Fe1Mn), Monel 400 (dissimilar), and weld overlay cladding onto steel tubesheets (over a pure nickel ERNi-1 buffer layer). |
| Supported Welding Processes | GTAW (TIG), GMAW (MIG / Pulsed) |
| Shielding Gas Recommendations | 100% Argon or Ar + He (GTAW & GMAW) |
| Available Wire Diameters | MIG Spools: 0.8mm (.030"), 0.9mm (.035"), 1.0mm (.040"), 1.2mm (.045"), 1.6mm (1/16") TIG Cut-Length Rods: 1.2mm, 1.6mm (1/16"), 2.0mm, 2.4mm (3/32"), 3.2mm (1/8"), 4.0mm (5/32") × 914mm (36") / 1000mm |
| Packaging & Storage | TIG Rods: 5 kg / 10 kg moisture-resistant tubular plastic packs in export master cartons. MIG Wire: 12.5 kg / 15 kg precision layer-wound BS300 / S200 spools sealed in VCI polyethylene film. Storage: Store in a dry, temperature-controlled indoor store (+10°C to +40°C, <60% RH) in original sealed packaging. |
Chemical Composition Specification (AWS A5.7 / ASME SFA-5.7 ERCuNi)
The table below specifies the standard wire chemical composition limits in weight percent (wt.%). Single values represent maximum permissible limits unless stated otherwise:
| Element | Verified Specification Limit (wt.%) | Metallurgical Function in Weld Metal |
|---|---|---|
| Copper (Cu) | Remainder (~66 – 69%) | Matrix base providing thermal conductivity and natural biofouling resistance |
| Nickel + Cobalt (Ni+Co) | 29.0 – 32.0 | Elevates strength and electrochemical nobility in flowing seawater |
| Iron (Fe) | 0.40 – 0.75 | Crucial for forming a tenacious erosion-corrosion-resistant oxide film |
| Manganese (Mn) | 1.00 max | Desulfurizer and weld pool fluidizer |
| Titanium (Ti) | 0.20 – 0.50 | Essential deoxidizer preventing gas porosity in arc welds |
| Silicon (Si) | 0.25 max | Controlled low silicon to prevent hot cracking |
| Lead (Pb) | 0.02 max | Strictly restricted to prevent grain-boundary hot shortness |
| Phosphorus (P) & Sulfur (S) | P ≤ 0.020, S ≤ 0.015 | Ultra-low impurities for ductile, crack-free multi-pass welds |
| Carbon (C) | 0.04 max | Low carbon limit |
Mechanical & Physical Properties
The values below distinguish between minimum AWS/ISO classification requirements for all-weld-metal test assemblies and typical as-welded deposited weld metal benchmarks:
| Property | Value | Unit | Specification / Reference Basis |
|---|---|---|---|
| Tensile Strength | ≥ 345 (Typical: 380 – 420) | MPa | AWS A5.7 ERCuNi Minimum / Typical Deposit |
| Yield Strength (0.2% Offset) | ≥ 140 (Typical: 170 – 210) | MPa | Typical As-Welded GTAW Deposit |
| Elongation | ≥ 30 (Typical: 35) | % | In 50 mm Gauge Length |
| Hardness | 85 – 105 | HB | Typical Deposited Weld Metal |
| Density | 8.94 | g/cm³ | Physical Property Reference |
| Melting Range | 1170 – 1240 | °C | Physical Property Reference |
Corrosion Resistance, Welding Considerations & Industrial Applications
Cupro Nickel 70/30 filler wire requires scrupulous joint cleanliness: remove all grease, cutting oils, oxide scale and shop markers for at least 25 mm on both sides of the bevel before welding, as sulfur, phosphorus or lead traces cause immediate intergranular cracking. Maintain interpass temperature below 150°C and use 100% Argon back-purging on single-sided seawater pipe root runs.
Typical Industrial Applications
- Multi-Stage Flash (MSF) and Multi-Effect Distillation (MED) seawater desalination evaporator shells, waterboxes and brine heaters
- Offshore oil & gas platform seawater cooling, firewater and ballast piping systems
- Naval submarine and surface warship high-pressure seawater piping and condenser tubesheets
- Marine shell-and-tube heat exchangers, power plant surface condensers and oil coolers
- Weld overlay cladding of carbon steel heat exchanger tubesheets and waterboxes
International Enquiry Destinations
FillerWires welcomes B2B export enquiries for Cupro Nickel 70/30 Filler Wire from EPC contractors, process equipment fabricators, shipyards and distributors across the following priority countries and industrial cities:
| Target Country | Relevant Industrial Cities & Ports | Typical Regional Sector Demand |
|---|---|---|
| United Arab Emirates | Abu Dhabi, Dubai, Sharjah, Fujairah, Jebel Ali | Desalination plants, offshore yards & drydock shiprepair |
| Oman, Qatar & Bahrain | Muscat, Sohar, Duqm, Salalah, Doha, Ras Laffan, Manama, Hidd | Coastal desalination, LNG cooling water & shipyards |
| Saudi Arabia & Kuwait | Jubail, Yanbu, Jeddah, Dammam, Ras Al-Khair, Shuwaikh, Shuaiba | SWCC desalination complexes & naval/offshore piping |
| Singapore & Sri Lanka | Jurong, Tuas, Pioneer, Colombo, Trincomalee, Galle | FPSO marine conversion & commercial shiprepair |
| Italy, Germany, UK & Netherlands | Genoa, Trieste, Venice, Hamburg, Southampton, Glasgow, Rotterdam | Cruise/naval shipbuilding & marine heat exchangers |
| United States, South Africa & Peru | Houston, San Diego, Norfolk, Durban, Cape Town, Callao | Naval dockyards, offshore rigs & coastal condensers |
Frequently Asked Questions — Cupro Nickel 70/30 Filler Wire
Technical questions and answers regarding classification, base metal compatibility, welding parameters and procurement for Cupro Nickel 70/30 Filler Wire:
Cupro Nickel 70/30 Filler Wire is classified under AWS A5.7 / ASME SFA-5.7 ERCuNi and EN ISO 24373 S Cu 7158 (CuNi30Mn1FeTi) (UNS UNS C71580 / C71581, Werkstoff Nr. 2.0837 (CuNi30Fe)). Contact us for confirmed product specifications and available technical documentation.
Cupro Nickel 70/30 Filler Wire (AWS A5.7 / ASME SFA-5.7 ERCuNi) is engineered for welding Copper-Nickel 70/30 (UNS C71500 / CuNi30Mn1Fe), Copper-Nickel 90/10 (UNS C70600 / CuNi10Fe1Mn), Monel 400 (dissimilar), and weld overlay cladding onto steel tubesheets (over a pure nickel ERNi-1 buffer layer).
Cupro Nickel 70/30 Filler Wire is supplied for GTAW (TIG), GMAW (MIG / Pulsed) as precision layer-wound MIG spools (0.8mm, 0.9mm, 1.0mm, 1.2mm, 1.6mm) and straight cut-length TIG rods (1.2mm, 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm in 914mm / 36-inch and 1000mm lengths). Recommended shielding gas: 100% Argon or Ar + He (GTAW & GMAW).
Cupro Nickel 70/30 filler wire requires scrupulous joint cleanliness: remove all grease, cutting oils, oxide scale and shop markers for at least 25 mm on both sides of the bevel before welding, as sulfur, phosphorus or lead traces cause immediate intergranular cracking. Maintain interpass temperature below 150°C and use 100% Argon back-purging on single-sided seawater pipe root runs. Typical applications include: Multi-Stage Flash (MSF) and Multi-Effect Distillation (MED) seawater desalination evaporator shells, waterboxes and brine heaters; Offshore oil & gas platform seawater cooling, firewater and ballast piping systems; Naval submarine and surface warship high-pressure seawater piping and condenser tubesheets.
International B2B Technical Enquiry & Quotation Request
Submit your alloy grade, AWS/ISO classification, diameter, welding process and delivery destination. Our technical export team in Mumbai responds to enquiries from the Middle East, GCC, USA, UK, Europe, Singapore, Sri Lanka, South Africa, Peru and global markets.