Hastelloy C276 Filler Wire Supplier — AWS A5.14 ERNiCrMo-4 Welding Wire
Low-carbon, low-silicon Nickel-Molybdenum-Chromium-Tungsten filler wire (AWS A5.14 ERNiCrMo-4 / UNS N10276) engineered for extreme chemical processing, wet chlorine, sour gas and flue-gas desulfurization (FGD) systems.
Universal Corrosion-Resistant Ni-Mo-Cr-W Filler Metal for Aggressive Chemical Service
Hastelloy C276 Filler Wire (classified under AWS A5.14 ERNiCrMo-4 / Alloy C276 Filler Metal) is a premier nickel-molybdenum-chromium-tungsten welding consumable universally recognized for its resistance to severe oxidizing and reducing chemical environments. High molybdenum (15.0–17.0%) and tungsten (3.0–4.5%) confer exceptional resistance to reducing acids (hydrochloric and sulfuric) and localized chloride pitting/crevice corrosion, while chromium (14.5–16.5%) protects against oxidizing media.
By restricting carbon (≤0.02%) and silicon (≤0.08%) to ultra-low levels, ERNiCrMo-4 suppresses grain-boundary carbide and intermetallic mu-phase precipitation in the weld heat-affected zone (HAZ), enabling components to be placed directly into corrosive service in the as-welded condition without post-weld solution annealing.
Alloy Identification, Standards & Supply Specifications
To preserve maximum corrosion resistance in the as-welded state, avoid excessive heat input and keep interpass temperatures below 95°C (200°F).
| Product Designation | Hastelloy C276 Filler Wire (TIG Welding Rod / MIG Spooled Wire) |
|---|---|
| AWS / ASME Classification | AWS A5.14 ERNiCrMo-4 |
| EN / ISO Classification | EN ISO 18274 S Ni 6276 (NiCr15Mo16Fe6W4) |
| UNS Designation & Werkstoff Nr. | UNS N10276 • W.Nr. 2.4819 |
| Compatible Base Materials | Alloy C276 (UNS N10276 / W.Nr. 2.4819), other Ni-Cr-Mo alloys, super-austenitic and super-duplex stainless steels, and corrosion-resistant weld overlay cladding on carbon or low-alloy steel vessels and flue-gas ducting. |
| Supported Welding Processes | GTAW (TIG), GMAW (Pulsed / Spray MIG) |
| Shielding Gas Recommendations | 100% Argon (GTAW); Argon + Helium (Pulsed GMAW) |
| Available Wire Diameters | MIG Spools: 0.8mm (.030"), 0.9mm (.035"), 1.0mm (.040"), 1.2mm (.045"), 1.6mm (1/16") TIG Cut-Length Rods: 1.2mm, 1.6mm (1/16"), 2.0mm, 2.4mm (3/32"), 3.2mm (1/8"), 4.0mm (5/32") × 914mm (36") / 1000mm |
| Packaging & Storage | TIG Rods: 5 kg / 10 kg moisture-resistant tubular plastic packs in export master cartons. MIG Wire: 12.5 kg / 15 kg precision layer-wound BS300 / S200 spools sealed in VCI polyethylene film. Storage: Store in a dry, temperature-controlled indoor store (+10°C to +40°C, <60% RH) in original sealed packaging. |
Chemical Composition Specification (AWS A5.14 ERNiCrMo-4)
The table below specifies the standard wire chemical composition limits in weight percent (wt.%). Single values represent maximum permissible limits unless stated otherwise:
| Element | Verified Specification Limit (wt.%) | Metallurgical Function in Weld Metal |
|---|---|---|
| Nickel (Ni) | Remainder (~57%) | Base matrix immune to chloride-induced stress-corrosion cracking |
| Molybdenum (Mo) | 15.0 – 17.0 | Primary defense against reducing acids and chloride pitting/crevice attack |
| Chromium (Cr) | 14.5 – 16.5 | Provides resistance to oxidizing acids, ferric/cupric salts and wet chlorine |
| Iron (Fe) | 4.0 – 7.0 | Controlled matrix alloying element |
| Tungsten (W) | 3.0 – 4.5 | Synergistically reinforces molybdenum against localized crevice corrosion |
| Cobalt (Co) | 2.5 max | Controlled solid-solution element |
| Carbon (C) | 0.02 max | Ultra-low carbon prevents grain-boundary carbide precipitation in the HAZ |
| Silicon (Si) | 0.08 max | Ultra-low silicon suppresses intermetallic phase formation |
| Manganese (Mn) & Vanadium (V) | Mn ≤ 1.0, V ≤ 0.35 | Deoxidation and minor alloying control |
| Phosphorus (P) & Sulfur (S) | P ≤ 0.040, S ≤ 0.030 | Strict impurity limits |
Mechanical & Physical Properties
The values below distinguish between minimum AWS/ISO classification requirements for all-weld-metal test assemblies and typical as-welded deposited weld metal benchmarks:
| Property | Value | Unit | Specification / Reference Basis |
|---|---|---|---|
| Tensile Strength | ≥ 690 (Typical: 750 – 810) | MPa | AWS A5.14 Minimum / Typical All-Weld-Metal |
| Yield Strength (0.2% Offset) | ≥ 415 (Typical: 460 – 510) | MPa | Typical As-Welded GTAW Deposit |
| Elongation | ≥ 25 (Typical: 35 – 40) | % | AWS A5.14 Minimum in 4D |
| Density | 8.89 | g/cm³ | Physical Property Reference |
| Melting Range | 1325 – 1370 | °C | Physical Property Reference |
Corrosion Resistance, Welding Considerations & Industrial Applications
Hastelloy C276 filler wire is one of the very few materials capable of withstanding wet chlorine gas, hypochlorite and chlorine dioxide solutions, as well as hot contaminated mineral acids, formic/acetic acids, acetic anhydride and sour gas wells containing high H2S, CO2 and elemental sulfur. Do not use oxy-acetylene or submerged arc welding (SAW) on C276, as high heat input and flux silicon/carbon pickup degrade corrosion resistance.
Typical Industrial Applications
- Chemical processing reactors, heat exchangers, columns and piping handling hydrochloric, sulfuric and organic acids
- Flue Gas Desulfurization (FGD) absorber tower linings (“wallpaper” cladding), outlet ducts and dampers in power plants
- Pulp and paper chlorine dioxide bleaching equipment and digesters
- Sour gas downhole tools, wellhead components and flare gas scrubbers (NACE MR0175 / ISO 15156)
- Pharmaceutical synthesis vessels and hazardous waste incineration scrubbers
International Enquiry Destinations
FillerWires welcomes B2B export enquiries for Hastelloy C276 Filler Wire from EPC contractors, process equipment fabricators, shipyards and distributors across the following priority countries and industrial cities:
| Target Country | Relevant Industrial Cities & Ports | Typical Regional Sector Demand |
|---|---|---|
| Saudi Arabia | Jubail, Yanbu, Dammam, Ras Al-Khair, Jazan | Petrochemical reactors, sour gas & acid processing plants |
| United Arab Emirates & Oman | Abu Dhabi, Ruwais, Dubai, Sohar, Duqm, Salalah | Sour gas processing, refinery scrubbers & chemical skids |
| Qatar, Kuwait & Bahrain | Ras Laffan, Mesaieed, Ahmadi, Shuaiba, Sitra | Sour gas treatment, sulfur recovery & desalination |
| United States & United Kingdom | Houston, Baton Rouge, Pittsburgh, Chicago, Teesside, Birmingham, Aberdeen | Chemical complexes, FGD scrubbers & oilfield equipment |
| Germany, Italy & Netherlands | Frankfurt, Ludwigshafen, Hamburg, Milan, Turin, Rotterdam | Chemical reactor & pressure vessel manufacturing |
| Singapore, South Africa & Peru | Jurong Island, Tuas, Johannesburg, Durban, Lima, Callao | Specialty chemicals, pharmaceutical & mining autoclaves |
Frequently Asked Questions — Hastelloy C276 Filler Wire
Technical questions and answers regarding classification, base metal compatibility, welding parameters and procurement for Hastelloy C276 Filler Wire:
Hastelloy C276 Filler Wire is classified under AWS A5.14 ERNiCrMo-4 and EN ISO 18274 S Ni 6276 (NiCr15Mo16Fe6W4) (UNS UNS N10276, Werkstoff Nr. 2.4819). Contact us for confirmed product specifications and available technical documentation.
Hastelloy C276 Filler Wire (AWS A5.14 ERNiCrMo-4) is engineered for welding Alloy C276 (UNS N10276 / W.Nr. 2.4819), other Ni-Cr-Mo alloys, super-austenitic and super-duplex stainless steels, and corrosion-resistant weld overlay cladding on carbon or low-alloy steel vessels and flue-gas ducting.
Hastelloy C276 Filler Wire is supplied for GTAW (TIG), GMAW (Pulsed / Spray MIG) as precision layer-wound MIG spools (0.8mm, 0.9mm, 1.0mm, 1.2mm, 1.6mm) and straight cut-length TIG rods (1.2mm, 1.6mm, 2.0mm, 2.4mm, 3.2mm, 4.0mm in 914mm / 36-inch and 1000mm lengths). Recommended shielding gas: 100% Argon (GTAW); Argon + Helium (Pulsed GMAW).
Hastelloy C276 filler wire is one of the very few materials capable of withstanding wet chlorine gas, hypochlorite and chlorine dioxide solutions, as well as hot contaminated mineral acids, formic/acetic acids, acetic anhydride and sour gas wells containing high H2S, CO2 and elemental sulfur. Do not use oxy-acetylene or submerged arc welding (SAW) on C276, as high heat input and flux silicon/carbon pickup degrade corrosion resistance. Typical applications include: Chemical processing reactors, heat exchangers, columns and piping handling hydrochloric, sulfuric and organic acids; Flue Gas Desulfurization (FGD) absorber tower linings (“wallpaper” cladding), outlet ducts and dampers in power plants; Pulp and paper chlorine dioxide bleaching equipment and digesters.
International B2B Technical Enquiry & Quotation Request
Submit your alloy grade, AWS/ISO classification, diameter, welding process and delivery destination. Our technical export team in Mumbai responds to enquiries from the Middle East, GCC, USA, UK, Europe, Singapore, Sri Lanka, South Africa, Peru and global markets.